Mechanical properties of Ti-6Al-4V(Ti Gr.5) Wires
Ti-6Al-4V Wires performance as specified by technical standards | |||||||||||
Type | State | δ or d /mm | Sampling direction | σb/MPa | Room temperature | 400℃ | |||||
τp02/MPa | δ5/% | φ/% | αKU/kJ·m-2 | α/(º) | σb/MPa | σ100/Mpa | |||||
≥ | |||||||||||
Wires | Annealed | 1.6~7.0 | L | ≥895 | - | 10 | - | - | - | - | - |
Hardness of Ti-6Al-4V(Ti Gr.5) Wires
- Room temperature hardness in annealed state HBS=255~341
- Room temperature hardness in solution aging state HBS=293~361